The product under the development

The two components are mixed together in a given proportion. After the kneading to homogenious state, shape the form, take a cast, apply to a destinct surface to rubberize it, or to the rubber surface to seal a crack. After 24 hours @room temperature or 2 minutes @80 Celsium degrees the mass will demonstrate the rubber properties and still be hardening hereafter. The product will be produced in both waterproof and oilproof modifications.

The product is at the prototype stage and still under the development.

The material is designed for a domestic use. Mixing is manual with no instrumental need.